18650 battery
This dataset presents the capacity fade data for eight Lithium Titanate Oxide (LTO) battery cells over progressive charge-discharge cycles. The measurements, recorded at intervals of 250 cycles up to 3500 cycles, track the aging effects on battery capacity over time. The aging procedure includes a rest period of 10 minutes between charging and discharging cycles. Each charging and discharging process was conducted with a constant current of 1 ampere (A). The maximum charge voltage was set to 2.75 volts (V), while the minimum discharge voltage was set at 1.30 V.
- Categories:
The dataset consists of results of 10 different tests conducted on 8 different types of battery cells. All batteries are designed in 18650, but they differ in manufacturer and composition. The measurements can be divided into three groups: constant load tests, WLTP tests at different temperatures and transient tests. Constant load tests are performed at 0.1C and 1C as a function of battery capacity, both during charging and discharging. During transient tests, a 360s load/charge is followed by a 60s relaxation.
- Categories: